研究表明,AlTiC系新型细化剂可使AlSiCu合金的铸态晶粒尺寸由4000~5000μm细化到200~300μm,共晶硅相的形状和尺寸由50μm×2μm的长条细化到1μm左右的圆点,合金力学性能明显提高
The results show that the Al-Ti-C series refiner can make the as-cast grain size of Al-Si-Cu alloy thinned from 4000-5000μm to 200-300μm, and the shape and size of the eutectic silicon phase from 50μm × 2μm Of the strip refinement to about 1μm dot, the mechanical properties of the alloy increased significantly