掌握了间歇逆流清洗中各清洗槽污物浓度的计算之后,就可以推算出在一定清洗条件下,什么时候应该换水,以及需要几个清洗槽。现举例说明如下:[例1]设原液污物浓度为50000mg/l,最后清洗槽允许污物的最大浓度为20mg/l。即要求 Co/C_末>2500。由于清洗零件不止一种,假设使用简单清洗条件,η可取0.9(在实际计算中可采用实测值)。(1)先考虑五级清洗由公式(Ⅳ)所算出的数据表及算图中可以查 Having mastered the calculation of the concentration of contaminants in each tank during intermittent counter-current cleaning, it is possible to figure out when it is time to change the water and how many tanks are required under certain conditions of cleaning. The following is an example: [Example 1] The concentration of the original liquid waste is 50000 mg / l, and the maximum allowable concentration of the dirt in the final washing tank is 20 mg / l. That is, Co / C_ end> ​​2500 is required. Since there are more than one part to be cleaned, assuming that a simple cleaning condition is used, η may be 0.9 (actual values ​​may be used in actual calculations). (1) first consider the five cleaning formula (Ⅳ) calculated by the data table and calculation can check
其他文献
马克思曾经阐述过资本主义条件下“土地级差地租”的产生及分配,同时也涉及到了矿山的级差地租问题.矿产资源的级差矿利与土地的级差地租相类似,即地质、地理及开采等条件较
本文研究了脉冲磁场对气体氮化的氮化层深度、化合物层厚度、氮化层组织及其硬度的影响。实验结果表明,脉冲磁场氮化后氮化层深度和化合物层厚度均大于常规氮化,氮化层中的氮
一、前言锻模寿命,系指一套锻模直至它不能使用为止(即翻新前)所生产的锻件数。自然,在锻模的使用过程中,应该包括必要的修理,修理就意味着该锻模可以继续使用。锻模寿命一
本文对硬质合金拉丝模渗硼工艺新技术进行了探讨。对硬质合金模渗硼后表面硬度、耐磨性及使用寿命的提高进行了研究。分析了硬质合金拉丝模磨损机理:模子的磨损是磨粒磨损和
铍青铜(QBe 2)具有优异的物理、机械性能,用于制造弹性元件、耐磨零件、换向开关以及在高速高温下工作的轴承、衬套,波纹管等。由于铍青铜的塑性很差,锻造比较困难,所以,我
随着高效、高速、高能量、大吨位的机械化、自动化锻压设备的发展以及冷挤、冷镦、冷冲等少无切削加工工艺的广泛应用,对模具的强度、韧性和耐磨性,提出了更高的要求。目前
本文研究了大晶粒铝锰β—黄铜材料的应变速率、变形温度及原始组织对超塑性拉伸时总延伸率的影响规律;确定了材料的m值,并计算了超塑性变形时的激活能。金属超塑性的研究工
本文通过磨粒磨损实验和磨损表面形貌分析,对65Mn钢表面硼共晶层的低应力磨粒磨损特性以及磨粒磨损机理进行了研究。研究表明:硼共晶组织经淬火后,具有优良的抗磨粒磨损性能
胡延品、尹登成此文登载于1988年《北京师范大学学报》第6期。文章说,台湾省重视发展教育。1980—1985年度。政府的教育经费支出占“国民生产总值(GNP)”的比率平均为4.3%,